热轧钢板 规格表
Hot Rolled Plate Specifications — 36个尺寸
KS D 3503JIS G 3101
KSJISHot Rolled Plate
12 sizes以下尺寸在 KS D 3503 · JIS G 3101 中相同。
| Nominal | t | Width | Length | Weight | Material |
|---|---|---|---|---|---|
| t1.6 | 1.6 | 914~1524 | 1829~6096 | 12.56 | SS400 |
| t2.0 | 2 | 914~1524 | 1829~6096 | 15.7 | SS400 |
| t2.3 | 2.3 | 914~1524 | 1829~6096 | 18.06 | SS400 |
| t3.2 | 3.2 | 914~1829 | 1829~6096 | 25.12 | SS400 |
| t4.5 | 4.5 | 914~2000 | 2000~12000 | 35.33 | SS400 |
| t6.0 | 6 | 914~2500 | 2000~12000 | 47.1 | SS400 |
| t9.0 | 9 | 914~2500 | 2000~12000 | 70.65 | SS400 |
| t12.0 | 12 | 1524~2500 | 3000~12000 | 94.2 | SS400 |
| t16.0 | 16 | 1524~2500 | 3000~12000 | 125.6 | SS400 |
| t19.0 | 19 | 1524~2500 | 3000~12000 | 149.15 | SS400 |
| t22.0 | 22 | 1524~2500 | 3000~12000 | 172.7 | SS400 |
| t25.0 | 25 | 1524~2500 | 3000~12000 | 196.25 | SS400 |
SS400、SPHC等热轧钢板(HR),高温轧制,通用于结构件、框架和机械底座。表面有氧化皮,厚度1.2~25mm。
实务注意事项
- 涂装前必须去除热轧钢板的氧化皮。在氧化皮上涂装会因附着力不良导致涂层脱落。
选型指南
通用热轧钢板。SS400/SPHC标准,用于结构件、框架和机座。表面有氧化皮,外观要求高时需使用冷轧钢板。厚度1.2–25mm。
主要特点
- KS D 3501 (SPHC/SPHD/SPHE),热轧t1.2–25 mm,表面氧化皮
- 比冷轧可生产更厚板材,分为结构用和冲压用
- 酸洗后可达SPCC级表面,价格竞争力强
主要应用领域
建筑钢板、汽车框架、船体、桥面板、罐体/压力容器壳体
常见问题
SS400和SPHC有什么区别?
SS400为结构用(以抗拉强度为准);SPHC为加工用(以化学成分+成形性为准)。需要结构强度选SS400,冲压/折弯为主选SPHC。