Ad
熱軋鋼板 規格表
Hot Rolled Plate Specifications — 36個尺寸
KS D 3503JIS G 3101
KSJISHot Rolled Plate
12 sizes以下尺寸在 KS D 3503 · JIS G 3101 中相同。
| Nominal | t | Width | Length | Weight | Material |
|---|---|---|---|---|---|
| t1.6 | 1.6 | 914~1524 | 1829~6096 | 12.56 | SS400 |
| t2.0 | 2 | 914~1524 | 1829~6096 | 15.7 | SS400 |
| t2.3 | 2.3 | 914~1524 | 1829~6096 | 18.06 | SS400 |
| t3.2 | 3.2 | 914~1829 | 1829~6096 | 25.12 | SS400 |
| t4.5 | 4.5 | 914~2000 | 2000~12000 | 35.33 | SS400 |
| t6.0 | 6 | 914~2500 | 2000~12000 | 47.1 | SS400 |
| t9.0 | 9 | 914~2500 | 2000~12000 | 70.65 | SS400 |
| t12.0 | 12 | 1524~2500 | 3000~12000 | 94.2 | SS400 |
| t16.0 | 16 | 1524~2500 | 3000~12000 | 125.6 | SS400 |
| t19.0 | 19 | 1524~2500 | 3000~12000 | 149.15 | SS400 |
| t22.0 | 22 | 1524~2500 | 3000~12000 | 172.7 | SS400 |
| t25.0 | 25 | 1524~2500 | 3000~12000 | 196.25 | SS400 |
SS400、SPHC等熱軋鋼板(HR),高溫軋製,通用於結構件、框架和機械底座。表面有氧化皮,厚度1.2~25mm。
實務注意事項
- 塗裝前必須去除熱軋鋼板的氧化皮。在氧化皮上塗裝會因附著力不良導致塗層脫落。
選型指南
通用熱軋鋼板。SS400/SPHC標準,用於結構件、框架和機座。表面有氧化皮,外觀要求高時需使用冷軋鋼板。厚度1.2–25mm。
主要特點
- KS D 3501 (SPHC/SPHD/SPHE),熱軋t1.2–25 mm,表面氧化皮
- 比冷軋可生產更厚板材,分為結構用和沖壓用
- 酸洗後可達SPCC級表面,價格競爭力強
主要應用領域
建築鋼板、汽車框架、船體、橋面板、罐體/壓力容器殼體
常見問題
SS400和SPHC有什麼區別?
SS400為結構用(以抗拉強度為準);SPHC為加工用(以化學成分+成形性為準)。需要結構強度選SS400,沖壓/折彎為主選SPHC。